Title:
Method for preparing an improved creosote wood preservative from a coal tar creosote
Abstract:
An improved creosote wood preservative that has a light color and that forms a non-sticky crud deposit is prepared from a coal tar creosote. The coal tar creosote is reacted with one or more of the following groups of neutral compounds: paraformaldehyde, trioxane; or nitrobenzene, nitrotoluene, nitroxylene, tris (hydroxymethyl) nitromethane; or aluminum, zinc or sulfur, to produce a reacted creosote. This reacted creosote is distilled to yield a distillate, which is the improved creosote wood preservative, and a pitch residue.
Do you think this is a good invention? Vote now:
Votes so far: For:(0) Against:(0) Other info:
Inventors:
Greco, Nicholas P. (Pittsburgh, PA, US) Webb, David A. (Valencia, PA, US)
Application Number:
547859
Filing Date: 1975-02-07 Publication_date: 1976-08-10 Assignee:
Koppers Company, Inc. (Pittsburgh, PA)
Primary Class(es):
106/18.31
106/18.33, 106/18.35, 106/18.36, 106/273.1, 106/284, 106/284.4, 208/2, 568/716
Other Classes:
US Patent Ref:
Other Refs:
Primary Examiner:
Thomas, Jr., James O.
Assistant Examiner:
Lone, W. B.
Attorney:
Brumback; Oscar B., Zeh, Jr.; Herbert J., Stachel; Kenneth J.
|
|

|